| Sign In | Join Free | My chinacomputerparts.com |
|
| Categories | Differential Scanning Calorimeter |
|---|---|
| Brand Name: | JINHAIHU |
| Model Number: | DSC-100A |
| Certification: | ISO 9001 |
| Place of Origin: | BEIJING, CHINA |
| MOQ: | 1 set |
| Payment Terms: | T/T,L/C,Western Union,MoneyGram,D/A,D/P |
| Supply Ability: | 20 sets per month |
| Delivery Time: | 7-15 working days |
| Packaging Details: | Conventional export wooden crates |
| Product name: | Differential Scanning calorimeter (DSC)Oxygen Induction Time (OIT) |
| Model: | DSC-100A |
| Certificate: | ISO, CE |
| DSC Range: | 0~±600mW |
| Temperature Range: | Room temperature ~ 600℃ Air cooling |
| Heating Rate: | 0.1~100 ℃/min |
| Temperature Resolution: | 0.01℃ |
| Temperature Fluctuation: | ±0.01℃ |
| Company Info. |
| Beijing Tonghe Testing Machine Co., ltd |
| Verified Supplier |
| View Contact Details |
| Product List |
Differential Scanning calorimeter (DSC)Oxygen Induction Time (OIT)
>Brief introduction of the instrument:
Differential scanning calorimetry (DSC) technique is widely applied. The differential scanning calorimeter serves as both a routine quality testing tool and a research instrument, measuring the temperature and heat flow associated with internal thermal transitions in materials. Our instrument is a heat flow type differential scanning calorimeter, featuring good repeatability and high accuracy, which is particularly suitable for precise specific heat measurement. The equipment is easy to calibrate, uses low - melting - point materials, is fast and reliable, and has a very broad application range, especially in material research and development, performance testing, and quality control. Material properties such as glass transition temperature, cold crystallization, phase transition, melting, crystallization, product stability, curing/crosslinking, oxidation induction period, etc., fall within the research scope of differential scanning calorimetry. Different models should be selected according to experimental parameters and requirements.
>Instrument use:
Measurement of curing reaction temperature and thermal effect in polymer materialsMeasurement of material phase transition temperature and thermal effectMeasurement of crystallization, melting temperature and thermal effect in polymer materialsGlass transition temperature testing of polymer materials, etc.
Reference standard:
GB / T 19466.2 – 2004 / ISO 11357-2:1999 Part 2: Determination of glass transition temperature;
GB / T 19466.3 – 2004 / ISO 11357-3:1999 Part 3: Determination of melting and crystallization temperature and enthalpy;
GB / T 19466.6 - 2009 / ISO 11357-3: 1999 Part 6: Determination of oxidation induction time (isothermal OIT) and oxidation induction temperature (kinetic OIT).
Technical parameter:
| DSC | DSC-100A Differential scanning calorimeters |
| DSC range | 0~±600mW |
| Temperature range | Room temperature~600℃ |
| Heat-up rate | 0.1~100℃/min |
| Temperature resolution | 0.01℃ |
| Temperature fluctuations | ±0.01℃ |
| Temperature reproducibility | ±0.1℃ |
| DSC accuracy | 0.001mW |
| DSC sensitivity | 0.01uW |
| Temperature control method | Heating up and constant temperature (automatic control of the whole program) |
| Curve scan | Heating up the scan |
| Air control | The instrument switches automatically |
| Display mode | The 24bit color 7-inch LCD touchscreen display is shown |
| Data interface | Standard USB interface |
| Instrument standards | Equipped with standard substances (tin), the user can correct the temperature and thermal enthalpy |
| Note | All technical indicators can be adjusted according to the user needs |





|