AISI 682 INCOLOY 901 AMS 5660 Sheet Steel NiFeCr12Mo W-Nr 2.4975 Superalloy

Categories Alloy Steel Plates
Brand Name: PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL
Model Number: NiFeCr12Mo, W-Nr 2.4975, AISI 682, Incoloy 901, AMS 5660, UNS N09901
Certification: SGS, TUV, BV, ISO, MTC
Place of Origin: China
MOQ: 500kg
Price: Negotiations
Payment Terms: T/T
Supply Ability: 50000KGS/Month
Delivery Time: Ex-stock for delivery: 3-7 days Production lead time: 30-60 days
Packaging Details: Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement
Characteristic: Heat and Corrosion-resistant
Heat treatment condition: +AT, +P, etc
Processing methods: Ground, Milled, etc
Available Shapes: Steel strip via cold rolled, Forging piece
Surface: Polished, Black,
Material Category: Austenitic Nickel-Based Alloys
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

AISI 682 INCOLOY 901 AMS 5660 Sheet Steel NiFeCr12Mo W-Nr 2.4975 Superalloy

AISI 682 INCOLOY 901 AMS 5660 Sheet Steel NiFeCr12Mo W-Nr 2.4975 Superalloy


Describe


Alloy 901 / 2.4975 is a nickel-chromium-molybdenum alloy containing titanium.


Size Range


Round bar / Wire rod (Diameter): 8.0 mm to 1000 mm

Square bar / Flat bar: 8.0 mm to 1000 mm

Forging piece: Stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.

Heavy/middle plate via hot rolled: T5 - 200 mm X W10 - 1000 mm X L1000-12000 mm

Sheet steel via cold rolled: T5 - 10 mm X W5 - 1000 mm X L1000 - 1000 mm

Steel strip via cold rolled: T0.5 - 8.0 mm X W10 - 200 mm X L (or in coil form)

Length: Fixed length or random length or based on the customer's special requirement.


Chemical Composition and standard


Incoloy 901/N90901/AISI 682

NiFeCr12Mo/2.4975AMS 5660
ASTM Udimet 901DIN EN 10095-2018SAE AMS 5660L-2015


C(%): ≤0.10
Si(%): ≤0.40
Mn(%): ≤0.50
P(%)≤: 0.040
S(%)≤: 0.030
Cr(%): 11.0~14.0
Ni(%): 41.0~43.5

Mo(%): 5.30~6.50

Ti(%): 2.20~2.75

B(%): 0.01~0.02

Al(%): ≤0.35

Cu(%): ≤0.50

Fe(%): Remainder


C(%): ≤0.10
Si(%): ≤0.60
Mn(%): ≤2.0
P(%)≤: 0.02
S(%)≤: 0.01
Cr(%): 11.0~14.0
Ni(%): 40.0~45.0

Mo(%): 5.0~7.0

Ti(%): 2.35~3.1

Co(%): ≤1.0

Al(%): ≤0.35

Fe(%): Remainder


C(%): ≤0.10
Si(%): ≤0.60
Mn(%): ≤1.0
P(%)≤: 0.030
S(%)≤: 0.030
Cr(%): 11.0~14.0
Ni(%): 40.0~45.0

Mo(%): 5.0~7.0

Ti(%): 2.35~3.10

B(%): 0.01~0.02

Co(%): ≤1.0

Al(%): ≤0.35

Cu(%): ≤0.50

Pd(%): ≤5 ppm

Bi(%): ≤0.3 ppm

Se(%): ≤3 ppm

Fe(%): Remainder




Mechanical Properties


Tensile strength, σb/Mpa: ≥175

Yield Point, σs/Mpa: ≥ 125

Elongation, δ/%: 15

Reduction of Area,ψ/%: ≥19


Applications


  • aviation industry
  • ship industry
  • Industrial Sector Gas Turbines

Contact us


If you are interested in our products or have any questions, please contact our team of engineers at
sales@ss-bars.com




China AISI 682 INCOLOY 901 AMS 5660 Sheet Steel NiFeCr12Mo W-Nr 2.4975 Superalloy factory
Send your message to this supplier
 
*From:
*To: Mianyang Baoheng New Material Technology Co.,Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0