| Sign In | Join Free | My chinacomputerparts.com |
|
| Categories | Turbine Blade Steel |
|---|---|
| Brand Name: | PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL |
| Model Number: | Waspaloy, UNS N07001, 2.4654, DIN NiCr20Co13Mo4Ti3Al, grade 685, ATG W1 |
| Certification: | SGS, TUV, BV, ISO, MTC |
| Place of Origin: | China |
| MOQ: | 800kg |
| Price: | Negotiations |
| Payment Terms: | T/T |
| Supply Ability: | 50000KGS/Month |
| Delivery Time: | Ex-stock for delivery: 3-7 days Production lead time: 30-60 days |
| Packaging Details: | Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement |
| Product Name: | NiCr20Co13Mo4Ti3Al W-Nr 2.4654 Superalloy |
| Characteristic: | Corrosion and Heat-Resistant |
| Heat treatment condition: | +A, +W, etc |
| Processing methods: | Peeled, Milled, etc |
| Available Shapes: | Tubing, Steel plate, etc |
| Surface: | Grinded, Black, etc |
NiCr20Co13Mo4Ti3Al W-Nr 2.4654 Superalloy Waspaloy UNS N07001 Steel Bar
Product Information
Waspaloy (UNS N07001) is a nickel-based superalloy that is capable of age-hardening and exhibits excellent strength at temperatures as high as 980°C. It is widely used as a forging material for the manufacture of gas turbine and aerospace components. Its strength is generally comparable to R41 alloy, and it outperforms the 718 alloy at temperatures above 650-705°C. Waspaloy is commonly used for high-temperature applications, particularly in gas turbines.
Size Range
Round bar / Wire rod (Diameter):8.0 mm to 500 mm
Square bar / Flat bar: 5.0 mm to 500 mm
Forging piece: Stepped shafts with flanks / discs /tubes /slugs
/donuts /cubes /other different shapes based on OEM.
Heavy/middle plate via hot rolled: T5 - 1000 mm X W8 - 1000 mm X
L800-12000 mm
Sheet steel via cold rolled: T5.0 - 8 mm X W5 - 1000 mm X L100 -
1000 mm
Steel strip via cold rolled: T0.5 - 8 mm X W10 - 1000 mm X L (or in
coil form)
Length: Fixed length or random length or based on the customer's
special requirement.
Chemical Composition and standard
| NiCr20Co13Mo4Ti3Al / 2.4654 | ATG W1 |
-- | EN 10302-2008 | -- |
C(%): 0.02~0.10 Cu(%): ≤0.5 Ti(%): 2.75~3.25 Co(%): 12.0~15.0 Al(%): 1.2~1.6 Fe(%): ≤2.0 Zr(%): 0.02~0.12 B(%): 0.003~0.01 | C(%): 0.02~0.10 Cu(%): ≤0.1 Ti(%): 2.80~3.30 Co(%): 12.0~15.0 Al(%): 1.2~1.6 Fe(%): ≤2.0 Zr(%): 0.02~0.08 B(%): 0.003~0.010 | C(%): ≤0.06 Ti(%): ≤3.0 Co(%): ≤13.0 Al(%): ≤1.25 Fe(%): ≤2.0 |

Waspaloy / UNS N07001 Mechanical Properties
Tensile strength, Rm/MPa: ≥ 1100
Yield strength, Rp/MPa: ≥ 760
Elongation/%: ≥ 20
Reduction of area, ψ/%: --
Impact, KV /J: --
Hardness, HBW: --
Applications
Waspaloy (UNS N07001) is commonly used for compressors and rotor discs, shafts, washers, seals, rings and casings, fasteners, and various other engine hardware, airframe components, and missile systems.