| Sign In | Join Free | My chinacomputerparts.com |
|
| Categories | Alloy Round Bar |
|---|---|
| Brand Name: | PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL |
| Model Number: | INCOLOY alloy 825 |
| Certification: | SGS,TUV,BV,ISO,MTC |
| Place of Origin: | China |
| MOQ: | Negotiations |
| Price: | Negotiations |
| Payment Terms: | T/T |
| Supply Ability: | 100000KGS/Month |
| Delivery Time: | Ex-stock for delivery: 3-7 days Production lead time: 45-55days |
| Packaging Details: | Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement |
| Product Name: | INCOLOY alloy 825 Alloy Round Bar |
| Grades: | INCOLOY alloy 825 |
| Processing methods: | Shot blasted,Cold working,Machined,etc |
| Surface: | Black,Grinding,Centreless Ground,etc |
| Profile: | Round Bar,Sheets Plates,Forging Piece,etc |
| Price Term: | Ex-work,FOB,DDU etc. |
INCOLOY alloy 825 Alloy Round Bar 825 Superalloy Round Bar 825 Round Bar 825 Bar
Description
Our company provides INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar.
All of INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.
Round bar / Wire rod (Diameter): 5.5mm to 800mm
Square bar / Flat bar: 3mm to 800mm
Heavy/middle plate via hot rolled: T6 - 200mm X W10 - 1500mm X L1000-12000mm
Steel strip via cold rolled: T0.1 - 3mm X W5 - 200mm X L (or in coil form)
Products Details
INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar
| Chemical Composition (weight%): | Mechanical Properties Under Final Heat Treatment: |
C (%): ≤ 0.04 Ti(%):≤1.00 Fe(%):≤30.0 | Condition: Solution annealed Tensile strength, σb/≥ MPa: 586 Yield strength, σ0.2/≥ MPa: 241 Elonghation, δ ≥(%): 30.0 |

Applications:
INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar,Tall oil distillation columns and equipments,etc


INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar
FAQ
Q: How do you control the quality?
A: We have professional inspectors to analyze the chemical composition of INCOLOY alloy 825 solution treated Alloy Round Bar 825 quenched and tempered Superalloy Round Bar 825 Peeled Round Bar 825 Hot rolled steel products Bar and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.
Q: Do you accept customization?
A: Yes. If you have special requirements for products or packaging,
we can make them for you.
Q: Can you accept trial orders?
A: Our MOQ is usually 1 ton. However, if you want to place an order
as the start of our cooperation, we can accept smaller quantities
at the first time. Of course, after the start, we will have further
and longer cooperation.
Q: How do I get samples?
A: Free samples are available for your inspection and testing,
DHL/FedEx/UPS accounts can be used for sampling, and the courier
fee is borne by you.

Wooden Pallet BOX,based on the customer's special requirement,Standard Seaworthy Package,etc
|