UNS R30188 Cobalt Base Superalloy AMS 5608, AMS 5801 Inconel 188 /Alloy 188

Categories Inconel alloy series
Place of Origin: Suzhou, China
Brand Name: AIWEN
Model Number: UNS R30188-Avril
MOQ: 10kg
Price: Available per request
Packaging Details: By customers' require
Delivery Time: 20-25days
Payment Terms: T/T
Supply Ability: 10000 kg per month
  • Haven't found right suppliers
  • Our buyer assistants can help you find the most suitable, 100% reliable suppliers from China.
  • And this service is free of charge.
  • we have buyer assistants who speak English, French, Spanish......and we are ready to help you anytime!
Submit Buying Request
  • Product Details
  • Company Profile

UNS R30188 Cobalt Base Superalloy AMS 5608, AMS 5801 Inconel 188 /Alloy 188

Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy

Specifications of Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy:

AMS 5608, AMS 5801
EN 2.4683
PWA 1042
UNS R30188
Werkstoff 2.4683

Features of Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy:

Strength and oxidation resistant to 2000°F
Good post-aging ductility
Resistant to sulfate deposit hot corrosion

Applications of Inconel 188 /Alloy 188 /UNS R30188 Cobalt Base Superalloy:

Gas turbine engine combustor cans
Spray bars
Flame-holders and afterburner liners
Product Tags:

alloy 2205

  

uns n10276 alloy

  

6061 alloy

  
China UNS R30188 Cobalt Base Superalloy AMS 5608, AMS 5801 Inconel 188 /Alloy 188 factory
Send your message to this supplier
 
*From:
*To: Suzhou Xunshi New Material Co., Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0